dc.description206 hojas : ilustraciones, 29 x 21 cm + CD-ROM 6040es_ES
dc.description.abstractResumen .- En este trabajo se busca diseñar una planta de concentración de Cu por flotación, a partir de un mineral del tipo pórfido que tiene una concentración de Cu de 0,58 % y de Fe 1,78 %, mediante el empleo de reactivos biodegradables de pirita como son los taninos de guarango (biopolimeros complejos) y en base a las propiedades del mineral, se realizó la selección de las condiciones optimas de flotación para obtener un concentrado colectivo de sulfuros probando valores de concentración de reactivos como son el amil xantato de potasio(Kax), aerofloat (208) y el aceite de pino, además de diferentes tiempo de molienda y flotación. Definidas las mejores condiciones de flotación colectiva, se logro obtener un concentrado de sulfuros con un contenido de Cu de 5,95 % a un d80=116µm y después de someterlo a una remolienda, se procedió a la flotación selectiva de Cu aplicando como reactivo depresor de pirita los taninos y cal por medio de una simulación de flotación continua que incluye tres etapas: desbaste, colección y afino; lográndose un producto con un 25% de Cu aplicando una concentración de taninos de 1 g/ kg a un tamaño de partícula d80 de 44 µm. El diseño de la planta se basa en circuitos de flotación con celdas Denver-sub A del tipo 24 para las etapas de afino y 30 en el desbaste y colección ya que proporcionan gran flexibilidad necesaria por las fluctuaciones de cabeza y el molino de bolas para tratar 2000 t/d se determinó de 4,3X6 m. Abstract .- This paper seeks to design a plant Cu concentration by flotation, from a porphyry ore having a concentration of 0.58% Cu and 1.78% Fe, by using biodegradable reactive pyrite tannins such as guarango (complex biopolymers) and based on the properties of the mineral, the selection of the optimum conditions of flotation was performed to obtain a collective sulphide concentrate testing reagent concentration values such as potassium amyl xanthate (kax), aerofloat (208) and pine oil, and several milling and flotation time. Defined the best conditions for collective flotation is able to obtain a concentrate of sulphides containing 5.95% Cu to a d80 = 116μm and after subjecting to a regrind, proceeded to the selective flotation of Cu applied as a depressant reagent tannins pyrite and lime by means of a continuous flotation simulation includes three stages: grinding, collection and refining; achieving a product with a 25% Cu applying a tannin concentration of 1 g / kg to a particle size d80 of 44 µm. The plant design is based on circuits Denver flotation cell sub-type A 24 for refining stage and 30 in the roughing and collection as they provide great flexibility required by changes in head and ball mill to treat 2000 t / d was determined 4,3X6 m.es_ES
dc.description.sponsorshipLozada López, Marcelo Salvador, directores_ES
dc.language.isospaes_ES
dc.publisherQuito, 2015.es_ES
dc.rightsopenAccess-
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/-
dc.subjectDiseño de plantases_ES
dc.subjectOperaciones unitariases_ES
dc.titleDiseño de una planta de concentración por flotación de calcopirita con depresores biodegradables de piritaes_ES
dc.typebachelorThesises_ES
Aparece en las colecciones:Tesis Ing. Química (IQUIM)

Ficheros en este ítem:
Fichero Descripción TamañoFormato 
CD-6040.pdfTesis completa3,74 MBAdobe PDFVisualizar/Abrir


Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.