dc.identifier.citationSánchez Rivadeneira, F.G.(2024). Recuperación de zinc de polvos de acería por lixiviación selectiva con ácido fosfórico o hidróxido de sodio. 42 páginas. Quito : EPN, 2024.es_ES
dc.identifier.otherT-MVE 1104/CD 13908-
dc.identifier.urihttp://bibdigital.epn.edu.ec/handle/15000/25289-
dc.descriptionLos polvos de acería generados por hornos eléctricos de fundición de acero son un peligro ambiental por el elevado contenido de metales como el zinc, hierro, plomo, entre otros, además por su reducido tamaño de partícula. Los polvos de acería se pueden valorizar por distintos métodos piro e hidrometalúrgicos. En el presente estudio se trabaja con polvos de acería que contienen 26,3% de Zn, 20,1% de Fe y 0,9 % de Pb en forma de compuestos como magnetita, zincita y franklinita principalmente. En este trabajo se propone recuperar el zinc por lixiviaciones ácidas (ácido sulfúrico y ácido fosfórico) y básicas (hidróxido de sodio), para una posterior recuperación de zinc metálico por electrólisis y fusión.es_ES
dc.description.abstractElectric Arc Furnace Dust (EAFD) is an environmental hazard due to their high content of metals such as zinc, iron, lead, among others, as well as their small particle size. EAFD can be valorized by different pyro and hydrometallurgical methods. In the present study, we work mainly with steel mill dust containing 26.3% Zn, 20.1% Fe, and 0.9% Pb in the form of magnetite, zincite, and franklinite compounds. The aim is to recover zinc by acid leaching (sulfuric acid and phosphoric acid) and basic leaching (sodium hydroxide), for subsequent recovery of metallic zinc by electrolysis and smelting. The leaching tests are performed in one and two stages, with and without heating at 80 °C. The acid concentrations used are 150 g L-1 and for sodium hydroxide 240 g L-1. The best leaching recoveries were 94% with sulfuric acid, 97% with phosphoric acid, and 80% with sodium hydroxide, using a two-stage process and heating (80 °C). Electrolysis with graphite anode and stainless-steel cathode gives the best recovery results of zinc deposited on the cathode which can be purified by fusion to 99% purity.es_ES
dc.language.isospaes_ES
dc.publisherQuito : EPN, 2024.es_ES
dc.rightsopenAccesses_ES
dc.subjectMETALURGIA EXTRACTIVAes_ES
dc.subjectLIXIVIACIÓN ÁCIDAes_ES
dc.subjectPOLVOS DE ACERÍAes_ES
dc.subjectZINC ÁCIDO FOSFÓRICOes_ES
dc.titleRecuperación de zinc de polvos de acería por lixiviación selectiva con ácido fosfórico o hidróxido de sodio.es_ES
dc.typemasterThesises_ES
Aparece en las colecciones:Tesis Maestría en Metalurgia Extractiva y Medio Ambiente (FIQA)

Ficheros en este ítem:
Fichero Descripción TamañoFormato 
CD 13908.pdf1,35 MBAdobe PDFVisualizar/Abrir


Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.